11. 斜頂與后面的柱位空間太小,斜頂在運動時會干涉到柱子,能移動這個柱子的位置嗎?
The angular lifter interferes with the boss during ejection. Please consider changing the position
of the boss.
12. 這個筋骨位膠厚太溥,而且高度偏高,注塑時很難填充這個筋位,可以增加這個筋骨位的厚度嗎?
The rib here is too thin and on the high side, so it will be difficult to fill here when we do the
injection, can you inrcease the thickness of this rib?
13. 你是想將此筋骨位的高度加高/減低嗎?加膠的位置我們將用銅公放電加深。但減膠的位置有兩種做
? ???法,1、做鑲件;2、燒焊;因為鑲件的底部有運水,我們簡單的做法是燒焊處理,你可以接受嗎?
Will you increase/decrease the material on this rib? We will use EDM if you add material, but there
are two option if you choose to decrease:1.Make inserts;2.Welding, because there is water in the
bottom of the insert, is that OK?
14. 這個樣板的筋骨位底部燒焦,是因為排氣不良,我們可以在筋骨位的中間增加一個鑲件。
This sample has been burned in the bottom because the venting is not good, we can add an insert in
the middle of the rib.
15. 重做鑲件大約需要5-6天時間,你能接受嗎?
It will take about 5 or 6 days to redo the insert, is that OK?
16. 產(chǎn)品的這個面我們已經(jīng)做了曬紋處理,如果需要加膠,這個面我們需要重新外發(fā)曬紋??赡苄枰獛滋斓臅r間
。
? ???所以我們直接以銅公放電的火花紋取代你要求的紋路,你可以接受嗎?
We have made the texture on this side, if we add material, it will take some days to remake the
texture by out-resourcing, so we suggest using the texture by EDM instead, is that OK?
17. 模具是用公制/英制的配件?需要備用件嗎?
Is this mold dimension measured in inches or meters? Does it need spare parts?
18. 模具上銘牌上的刻字內(nèi)容是由你們提供嗎?你們什么時候可以這些刻字資料。
Will you provide the engraving content of the plate of this mold to us? When will you send it?
19. 可否提供此模具生產(chǎn)時,注塑機(jī)的型號及相關(guān)資料。如:啤機(jī)大小、呵林柱尺寸、頂棍孔尺寸等
Can you provide the type of injection machine and other related information of this mold to us?
Such as the boss dimension, the hole's dimension of the ejector pin and the size of the injection
machine and so on.
20. 這個問題我需要同其它同事商議會再答復(fù)你。
I need to discuss this problem with the other colleagues and then I will reply back to you.
?